MarkeTech Yttrium aluminum garnet:Ce (YGA:Ce; Y3Al5O12) Scintillator Crystal

Category Ceramic , Oxide
Manufacturer MarkeTech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MarkeTech Yttrium aluminum garnet:Ce (YGA:Ce; Y3Al5O12) Scintillator Crystal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Yttrium aluminum garnet activated by cerium is fast with excellent mechanical properties and is chemically resistant scintillator. Mechanical properties enable to produce YAG:Ce scintillation screens down to a thickness of 30 µm. YAG:Ce detectors are excellent for electron microscopy, beta and X-ray counting, electron and X-ray imaging screens.Data provided by the supplier, MarkeTech International.
Physical Properties Metric English Comments
Density 4.57 g/cc
0.165 lb/in³
Mechanical Properties Metric English Comments
Hardness, Mohs 8.5
8.5
Thermal Properties Metric English Comments
CTE, linear 8.00 - 9.00 µm/m-°C
4.44 - 5.00 µin/in-°F
Melting Point 1970 °C
3580 °F
Descriptive Properties Value Comments
Crystal Structure Cubic
Hydroscopic? No
Luminescence: Afterglow <0.005%
at 6 ms
Luminescence: Decay Constant 70 n/s
Luminescence: Integrated Light Output 15
NaI:Tl = 100
Luminescence: Photon Yield 8
300K; 10<sup>3</sup> pH/MeV
Luminescence: Radiation Length 3.5 cm
Luminescence: Wavelength of max emissions 550 nm