Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1750 - 1765 °C | 3180 - 3209 °F | |
Johnson Matthey HC Platinum w/ 5% Cobalt Jewelry Alloy Fluid for hard castings. Cobalt has been used to create casting alloys at various levels of fineness. Cobalt suppresses oxygen level in the melt, improves fluidity and castability and gives a good .. |
|||
Melting Point | 1755 - 1765 °C | 3191 - 3209 °F | |
Johnson Matthey SC 950 Platinum w/ 5% Palladium Jewelry Alloy Castings, delicate settings. Palladium has been used to create casting alloys at various levels of fineness. Palladium produces a softer casting. |
|||
Melting Point | 1750 - 1765 °C | 3180 - 3209 °F | |
Wieland 1746 Wilaform Platinum Platinum alloy particularly suitable for decoration castingApplications: casting, laminar decoration, tubingDental |