Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1755 - 1765 °C | 3191 - 3209 °F | |
Johnson Matthey SC 950 Platinum w/ 5% Palladium Jewelry Alloy Castings, delicate settings. Palladium has been used to create casting alloys at various levels of fineness. Palladium produces a softer casting. |