Thermal Properties Metric English Comments
Melting Point 146 °C
295 °F
Flow temperature, ASTM D569-59
Rotuba 856, Slow Burning Ethyl Cellulose
Data provided by the manufacturer.
Melting Point 146 - 165 °C
295 - 329 °F
Average value: 162 °C Grade Count:21
Overview of materials for Polypropylene, Fiber Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app..
Melting Point 146 - 161 °C
295 - 322 °F
TMA Melt Range, 25 mil film
Huntsman IROGRAN® A 85 P 5004 TPU-Polyether
IROGRAN® A 85 P 5004 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications.Information provided by Alliance Polymers
Melting Point 146 - 176 °C
295 - 349 °F
Indium Corp. Indalloy 102 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Melting Point 146 °C
295 °F
Techmer ES Plastiblend® TPX-HTN-000AA
Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc.
Melting Point 146 °C
295 °F
Techmer ES Plastiblend® TPX-HTN-000AB 15% Glass Filled
Availability: North AmericaForms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: High Heat ResistanceInformation provided by TP Composites, Inc.
Melting Point 146 °C
295 °F
ISO 3146
Total PPR 7220 Random Copolymer Polypropylene, Injection Molding
Total Petrochemicals PPR 7220 is a nucleated random copolymer polypropylene with a melt flow index of 10 g/10 min for the injection molding of articles with high transparency and excellent surface a..
Melting Point 146 °C
295 °F
ISO 3146
Total PPR 7227 Random Copolymer Polypropylene, Injection Molding
Total Petrochemicals PPR 7227 is a high transparency random copolymer polypropylene specially developed for the injection molding of caps and closures and articles with high transparency, excellent ..
Melting Point 146 °C
295 °F
DSC
Total PPR 7860 Controlled Rheology Grade Propylene Copolymer for Spunbond Nonwoven Fabrics, Multifilament Yarns and Extrusion Coating
TOTAL Petrochemicals Polypropylene 7860 is a propylene copolymer grade with narrow molecular weight distribution.Process Stability. 7860 features excellent processability and gas fade resistance.F..
Melting Point 146 °C
295 °F
ISO 3146
Total PPR 9220 Random Copolymer Polypropylene, Injection Molding
Total Petrochemicals PPR 9220 is a nucleated random copolymer polypropylene with a melt flow index of 20 g/10 min for the injection molding of articles with high transparency and excellent surface a..
Melting Point <= 146 °C
<= 295 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Escorene™ UL 7711 Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra UL 7711 is a very high flow, 26.7% VA copolymer that has very good compatibility with hydrocarbon and natural tackifiers and most waxes. It is suitable for making..
Melting Point 146 °C
295 °F
BASF Novolen® 3225 MC Polypropylene
Grade containing slip and blocking agents, for cast film with medium slip.Data was collected by ISO methods and provided by BASF.
Melting Point 146 °C
295 °F
BASF Novolen® 3236 MC Polypropylene
Grade containing slip, blocking and antistatic agents, for cast film with medium slip.Data was collected by ISO methods and provided by BASF.
Melting Point 146 - 154 °C
295 - 309 °F
DSC Induction Temperature; TM-029
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets
Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc...
Melting Point 146 - 154 °C
295 - 309 °F
DSC Induction Temperature; TM-029
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets
Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc...
Melting Point 146 °C
295 °F
AIM 97In/3Ag Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.