Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Plastiblend® TPX-HTN-000AB 15% Glass Filled

Category Polymer , Thermoplastic , Nylon , High Temperature Nylon
Manufacturer Techmer ES
Trade Name Plastiblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plastiblend® TPX-HTN-000AB 15% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: High Heat ResistanceInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
Water Absorption 3.1 %

@Time 86400 sec
3.1 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0075 cm/cm

@Thickness 3.17 mm
0.0075 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 124 MPa
18000 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 172 MPa
25000 psi
ASTM D790
Flexural Modulus 5.52 GPa
800 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm
1.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 64.8 µm/m-°C
36.0 µin/in-°F
ASTM D696
Melting Point 146 °C
295 °F
Maximum Service Temperature, Inert 160 °C
320 °F
ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 249 °C
480 °F
Unannealed; ASTM D648