Polymer Property : Melting Point = 253.8 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 123.2 °C
253.8 °F
DSC
Silon Tabond 3042 Impact Modifier for PA
Tabond 3042 is a chemically modified Ethylene Copolymer/LLDPE.Information provided by Silon