Polymer Property : Melting Point = 229 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 229 °C
444 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)
Unreinforced Renewably Sourced Polytrimethylene Terephthalate with Excellent Impact Resistance Sorona MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably..
Melting Point 229 °C
444 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably sourced ingredients by weight. It was initially coded SE38001.Information provided by DuPont..