Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1115 °C
2039 °F
Indium Corp. Germanium Corporation® GeO2 Germanium Dioxide
Germanium dioxide is a white powder that is manufactured in both crystalline and amorphous forms. Germanium dioxide's refractive index (1.7) and its optical dispersion properties are useful for mak..