Thermal Properties Metric English Comments
Melting Point 198 °C
388 °F
ISO METHOD 3146C
NYCOA 2061 Copolymer Nylon 6/69
monofilament weed eater, fishing lineInformation provided by NYCOA, Inc.
Melting Point 198 - 208 °C
388 - 406 °F
Temperature range at which MFI = 10 g/10 min at 21.6 kg.; MQSA 111
Lubrizol Advanced Materials Pearlthane® 11T75D Thermoplastic Polyurethane Elastomer
Pearlthane® 11T75D is a polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, with extremely high hardness. It is especially recommended for use in producin..
Melting Point <= 198 °C
<= 388 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Escorene™ UL 00014 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 00014 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic..