Polymer Property : Melting Point = 1793 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1793 °C
3259 °F
Unifrax Fiberfrax® 550 Ceramic Fiber Paper
550 paper is made from unwashed high-purity ceramic fiber. Its higher density and binders give performance properties ideal for most refractory applications.Information Provided by Unifrax I LLC
Melting Point 1793 °C
3259 °F
Unifrax Fiberfrax® 972-H Ceramic Fiber Paper
This product is completely free of organics and used when higher fired strength is required or in processes and applications where even small amounts of organic burnout is unacceptable. 972-H is he..
Melting Point 1793 °C
3259 °F
Unifrax Fiberfrax® 970 Ceramic Fiber Paper
970 paper is made from high-purity Fiberfrax washed fiber. During the manufacture of this product, a large portion of the unfiberized particles in the bulk fiber are removed prior to paper lay-up. ..