Polymer Property : Melting Point = 154 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 58.0 - 68.0 °C
136 - 154 °F
Fine Organics FINALUX G 748 Lubricant Additive
Applications: External lubricant and release agent for PVC, Polycarbonate, PET/PBT and ABS.Information provided by Fine Organics
Melting Point 64.0 - 68.0 °C
147 - 154 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 100 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 100 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity leve..
Melting Point 64.0 - 68.0 °C
147 - 154 °F
Kolfer; MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 120 Linear Thermoplastic Polyurethane
Pearlbond® 120 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticity ..
Melting Point 64.0 - 68.0 °C
147 - 154 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 500 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 500 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a high crystallization rate and a very high thermoplasticity level.Appli..
Melting Point 64.0 - 68.0 °C
147 - 154 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 520 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 520 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level...