Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 64.0 °C | 147 °F | Exxon Method |
ExxonMobil Optema® TC-221 Ethylene Methyl Acrylate for Compounding
(discontinued **) Data provided by the manufacturer, Exxon Chemical.27% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used for making alloys, blends, and compounds, or be injection molded where.. |
|||
Melting Point | 64.0 °C | 147 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® E403 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Melting Point | 64.0 °C | 147 °F | Freezing Point, DSC; ASTM D3418 |
DuPont Bynel® 21E553 Adhesive Resin
(discontinued **) Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in.. |
|||
Melting Point | 64.0 °C | 147 °F | Exxon Method |
ExxonMobil Escorene® LD-752 EVA Copolymer for Specialty Applications
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymer.Applications: Compound viscosity modifier; High flow applications. |
|||
Melting Point | 64.0 °C | 147 °F | Exxon Method |
ExxonMobil Escorene® UL-7720 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Melting Point | 64.0 - 68.0 °C | 147 - 154 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 100 Linear Thermoplastic Polyurethane Pearlbond™ 100 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity leve.. |
|||
Melting Point | 64.0 - 68.0 °C | 147 - 154 °F | Kolfer; MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 120 Linear Thermoplastic Polyurethane Pearlbond® 120 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticity .. |
|||
Melting Point | 64.0 - 68.0 °C | 147 - 154 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 500 Linear Thermoplastic Polyurethane Pearlbond™ 500 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a high crystallization rate and a very high thermoplasticity level.Appli.. |
|||
Melting Point | 64.0 - 68.0 °C | 147 - 154 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 520 Linear Thermoplastic Polyurethane Pearlbond™ 520 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level... |
|||
Melting Point | 64.0 °C | 147 °F | |
ChevronTexaco Compound L Rust Proof Texaco Rust Proof Compounds deliver value through:Excellent long-term rust protection — Petrolatum and special additive system form a nonhardening, self sealing film to protect surfaces against the.. |
|||
Melting Point | 63.9 °C | 147 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Escorene® LD 713.93 Blown Film Resin Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer film resin. Film made from LD 713.93 exhibits very high impact strength, high clarity, and excellent heat sealability.Availability: Lat.. |
|||
Melting Point | 64.0 °C | 147 °F | Freezing Point; ASTM D3418 |
DuPont™ Bynel® 21E533 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Melting Point | 64.0 °C | 147 °F | Freezing Point; ASTM D3418 |
DuPont™ Entira® ASSD100 Ionomer Resin DuPont™ Entira™ AS SD100 is an extremely hygroscopic ionomer resin that is supplied as free flowing pellets. Entira™ AS SD100 is used to lower the static decay time and surface resistivity of LD.. |
|||
Melting Point | 64.0 °C | 147 °F | DSC |
Arkema Group EVATANE® 33-15 Copolymer Ethylene - Vinyl Acetate EVATANE® 33-15 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-15 is stabilized with antioxidants. The High Vinyl Acetate co.. |
|||
Melting Point | 64.0 - 95.0 °C | 147 - 203 °F | Average value: 78.8 °C Grade Count:8 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Compounding Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Compounding Grade". Each property range of values reported is minimu.. |
|||
Melting Point | 64.0 °C | 147 °F | Exxon Method |
ExxonMobil Iotek® 7310 Zinc Ionomer
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low melt index zinc ionomer made from an ethylene acrylic acid base polymer.Applications: Injection molding; Impact modifier of polyamide. |
|||
Melting Point | 64.0 °C | 147 °F | Freezing Point; ASTM D3418 |
DuPont Surlyn® 1702SBR
(discontinued **) DuPont™ Surlyn® 1702SBR is a zinc-type resin made from ethylene/methacrylic acid copolymer. This resin has slip, antiblock, and chill roll release additives included in the resin to reduce the coe.. |