Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1480 - 1530 °C | 2700 - 2790 °F | |
Crucible Steel 410 Chromium Steel Crucible 410 is a hardenable chromium steel which is adaptable for general purpose corrosion resisting and heat resisting applications. This grade is magnetic at times. Information provided by Cruci.. |
|||
Melting Point | 1480 - 1530 °C | 2700 - 2790 °F | |
Crucible Steel 416 Plus Chromium Steel Crucible 416 Plus is a hardenable chromium steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of standard AISI Type 4.. |
|||
Melting Point | 1480 - 1530 °C | 2700 - 2790 °F | |
ATI Allegheny Ludlum Stainless Steel AL 410S™ (UNS S41008) Allegheny Ludlum Al 410S™ stainless steel is a low-carbon modification of Type 410 stainless steel. Low carbon and optionally a small addition of titanium and /or columbium minimize austenite form.. |