Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 67.0 °C | 153 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 2014 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Melting Point | 67.0 °C | 153 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 3062 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 67.0 °C | 153 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® E326 Acid-/Acrylate-Modified EVA Adhesive Resin
(discontinued **) Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce.. |
|||
Melting Point | 67.0 °C | 153 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Elvax® 3174SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Cast Film
(discontinued **) 18 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Melting Point | 67.0 °C | 153 °F | Exxon Method |
ExxonMobil Escorene® LD-781 High EVA Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 33% vinyl acetate copolymer for specialty compounding applications. The resin provides excellent stress cracking and flexibility, and allows outs.. |
|||
Melting Point | 67.0 °C | 153 °F | Exxon Method |
ExxonMobil Iotek® 7510 Zinc Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A "soft" zinc ionomer with excellent flexibility and impact strength. This ionomer has outstanding adhesion to glass, metals and paper. IOTEK iono.. |
|||
Melting Point | 67.0 °C | 153 °F | Exxon Method |
ExxonMobil Iotek® 7520 Zinc Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A "soft" zinc ionomer with excellent flexibility and impact strength. This ionomer has outstanding adhesion to glass, metals and paper. IOTEK iono.. |
|||
Melting Point | 67.0 °C | 153 °F | Freezing Point, DSC; ASTM D3418 |
DuPont Bynel® 3126 Adhesive Resin Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce.. |
|||
Melting Point | 67.0 °C | 153 °F | DSC, 10°C/min; DuPont Test |
Dow Engage® 8452 Polyolefin Elastomer Description: Engage® 8452 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent toughness, softness, and optical properties. It has excellent compatibility with other polyolefin.. |
|||
Melting Point | 67.0 °C | 153 °F | D.S.C. method |
Arkema Group Orevac® 9305 Film EVA-MAH Terpolymer EVA Terpolymers based Main Application: Hot melt adhesivesInformation provided by Arkema Group |