Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Bynel® 3126 Adhesive Resin

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Bynel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Bynel® 3126 Adhesive Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resinsApplications:Bynel® 3126 adheres to a wide variety of materials. It is most often used to adhere to PE, acid copolymers, and ionomers. The use of Bynel® Series 3100 resins can be advantageous in applications where acid-containing polymers, such as acid copolymers or ionomers, are to be combined with PVDC.Bynel® Series 3100 resins can be used in coextrusion processes including:blown filmcast film/sheetextrusion coatingthermal laminationPhysical properties Bynel® Series 3100 resins are typical of EVA resins with similar density and melt index values. The rheology characteristics of each grade are different, so one may be better suited than the others for a particular extrusion process.Information provided by DuPont™
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ASTM D792
Melt Flow 8.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 67.0 °C
153 °F
Freezing Point, DSC; ASTM D3418
87.0 °C
189 °F
DSC; ASTM D3418
Vicat Softening Point 60.0 °C
140 °F
ASTM D1525
Processing Properties Metric English Comments
Rear Barrel Temperature 120 °C
248 °F
Middle Barrel Temperature 220 °C
428 °F
Front Barrel Temperature 235 °C
455 °F
Adapter Temperature 235 °C
455 °F
Die Temperature 235 °C
455 °F
Copyright © lookpolymers.com All Rights Reserved