Thermal Properties Metric English Comments
Melting Point 147 - 151 °C
297 - 304 °F
M Chemical GUARD DOGâ„¢ UV1577 Light Absorber, Triazene Derivative
GUARD DOG™ UV1577 UV absorber is a low volatile Triazine based UV absorber which is highly effective in polymers that are processed at high temperature (decomposition temperature > 350°C).Ap..
Melting Point 143 - 151 °C
289 - 304 °F
Indium Corp. Indalloy 225 Indium Solder Alloy