Polymer Property : Melting Point = 1466 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1466 °C
2671 °F
Liquidus
AGY ZenTron® S-2 Generic S-Glass Fiber
S-2 glass and S-glass have the same composition. S-glass is no longer made by AGY, but used to have a reactive epoxy size. Various silanes and starch oil are used as binders. Acid resistant. Mod..