Thermal Properties Metric English Comments
Melting Point 671 - 779.4 °C
1240 - 1435 °F
Lucas-Milhaupt BRAZE 403 Carbide Brazing Alloy
Applications: Braze 403 is a good intermediate temperature brazing alloy for use on stainless steels, mild steels, cast and malleable irons and various nonferrous alloys. This alloy is particularly..
Melting Point 640.6 - 779.4 °C
1185 - 1435 °F
Lucas-Milhaupt SIL-FOS 2 Silver/ Copper/ Phosphorus Alloy
Applications: Sil-Fos 2 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encountered in servi..