Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 670 - 710 °C | 1240 - 1310 °F | |
Johnson Matthey Argo-braze 49LM Silver Brazing Alloy for Tungsten Carbide Brazing This material is supplied as Trifoil. Trifoil consists of a layer of copper sandwiched by brazing alloy. The copper helps to absorb the stresses caused by the differential expansion rates, under he.. |
|||
Melting Point | 671 - 779.4 °C | 1240 - 1435 °F | |
Lucas-Milhaupt BRAZE 403 Carbide Brazing Alloy Applications: Braze 403 is a good intermediate temperature brazing alloy for use on stainless steels, mild steels, cast and malleable irons and various nonferrous alloys. This alloy is particularly.. |
|||
Melting Point | 671 - 718.3 °C | 1240 - 1325 °F | |
Lucas-Milhaupt BRAZE 650 (Easy) Silver Based Cadmium Free Filler Metal Characteristics: This alloy is a intermediate silver brazing filler metals with a slight tendency to liquate (i.e. separate into low and high melting constituents) if heated slowly through their mel.. |