Polymer Property : Melting Point = 1420 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1420 °C
2590 °F
Goodfellow Nickel 92/Manganese 8 Alloy
Information provided by Goodfellow.
Melting Point 1420 °C
2590 °F
Goodfellow T1-Thermocouple Alloy
The positive element of the type K thermocouple alloy the negative being T2. The thermocouple can be used up to 1250C in oxidizing atmospheres and is the probably the most common in use. It is also ..