Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1250 - 1315 °C | 2280 - 2399 °F | |
Reade Advanced Materials Garnet Powder (Fe3Al2(SiO4)3) Description: A group of iron aluminum silicate homogeneous minerals having similar properties. Non-hygroscopic, sharp angular shape, inert, slightly magnetic, not soluble in water, translucent, fria.. |
|||
Melting Point | 1150 - 1315 °C | 2100 - 2399 °F | |
Materion Beryllium Nickel M220C Information supplied by Brush Wellman Engineered Materials.Brush M220C is characterized by high levels of strength, hardness, and thermal conductivity combined with excellent resistance to wear, cor.. |