Polymer Property : Melting Point = 1270 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1270 - 1395 °C
2320 - 2543 °F
Kennametal Stellite Denertiaâ„¢ C13 Cobalt Chromium Dental Alloy
Denertiaâ„¢ C13 is a cobalt chromium base-metal casting alloy for the manufacture of removable partial dentures and bridgework.This alloy is Nickel, Beryllium and Cadmium free as defined in ISO 6..
Melting Point 1270 °C
2320 °F
Universal Wire Works No. 6 Cobalt Alloy Welding Wire
Universal No. 6 is a cobalt-chromium-tungsten alloy suited for applications requiring extreme impact resistance at elevated temperatures, exhaust valve contact surfaces, hot and cold trimmer dies an..
Melting Point 1270 °C
2320 °F
Alloy Wire International RW 45 Ni-Cu Resistance Wire
Used in thermocouples, power resistors, shunts, and wire wound precision restors up to 750°F (400°C)Information provided by Alloywire International.