Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1171 °C | 2140 °F | Liquidus |
AGY ADVANTEX® Generic Glass Fiber OC/AGY E-CR glass. Various silanes and starch oil are used as binders. Acid resistant. Lower alkali resistance than VeTron® and ZenTron® glass fibers.Information provided by AGY Holding Corp... |