Polymer Property : Melting Point = 1085 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1085 - 3410 °C
1985 - 6170 °F
CMW® ELKONITE® 10W3 Copper Tungsten RWMA Class 11
Electrical contacts resistant to arcing, power transformer switches, resistance / projection welding electrodes, and EDM electrodesInformation provided by CMW Inc.
Melting Point 1085 - 3410 °C
1985 - 6170 °F
CMW® ELKONITE® 1W3 Copper Tungsten RWMA Class 10
Uses: Arcing and current carrying electrical contacts. Resistance/projection welding electrodes.Information provided by CMW Inc.
Melting Point 1085 - 3410 °C
1985 - 6170 °F
CMW® ELKONITE® 2050C Copper Tungsten Contact Material ASTM B702, Class A, infiltrated
Uses: Arcing and current carrying electrical contacts. Information provided by CMW Inc.