Polymer Property : Transformation Temperature = 288 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature 142 - 151 °C
288 - 304 °F
Temp at Max Expansion
Akzo Nobel Expancel® 051 WU 40 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Transformation Temperature 142 - 150 °C
288 - 302 °F
Temp at Max Expansion
Akzo Nobel Expancel® 461 DU 40 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Transformation Temperature 142 - 150 °C
288 - 302 °F
Temp at Max Expansion
Akzo Nobel Expancel® 461 WU 40 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Transformation Temperature 142 - 151 °C
288 - 304 °F
Temp at Max Expansion
Akzo Nobel Expancel® 051 DU 40 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..