Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | 142 - 151 °C | 288 - 304 °F | Temp at Max Expansion |
Akzo Nobel Expancel® 051 WU 40 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Transformation Temperature | 142 - 150 °C | 288 - 302 °F | Temp at Max Expansion |
Akzo Nobel Expancel® 461 DU 40 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Transformation Temperature | 142 - 150 °C | 288 - 302 °F | Temp at Max Expansion |
Akzo Nobel Expancel® 461 WU 40 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Transformation Temperature | 142 - 151 °C | 288 - 304 °F | Temp at Max Expansion |
Akzo Nobel Expancel® 051 DU 40 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |