Thermal Properties Metric English Comments
Transformation Temperature -40.0 - -2.00 °C
-40.0 - 28.4 °F
Average value: -8.54 °C Grade Count:13
Overview of materials for Thermoset Fluoroelastomer
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr..