Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | -40.0 °C | -40.0 °F | TR10; ASTM D1329 |
3M Dyneon™ LTFE 6400Z Low Temperature Fluoroelastomer 3M™ Dyneon™ Low Temperature Fluoroelastomers LTFE 6400Z are technically advanced low temperature, peroxide-cured fluoroelastomers, designated as a FKM type 3 elastomer per ASTM D1418. They are des.. |
|||
Transformation Temperature | -40.0 °C | -40.0 °F | TR10; ASTM D1329 |
3M Dyneon™ LTFE 6400ZC Low Temperature Fluoroelastomer 3M™ Dyneon™ Low Temperature Fluoroelastomers LTFE 6400ZC are technically advanced low temperature, peroxide-cured fluoroelastomers, designated as a FKM type 3 elastomer per ASTM D1418. They are de.. |
|||
Transformation Temperature | -40.0 - -2.00 °C | -40.0 - 28.4 °F | Average value: -8.54 °C Grade Count:13 |
Overview of materials for Thermoset Fluoroelastomer This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr.. |