Thermal Properties Metric English Comments
Transformation Temperature 555 °C
1030 °F
Ferro CF 7574 Glaze and Sealant Glass
Glass Type: Zn-B-Si Typical Powder Form: VSD Typical Application: Pyrex Silicon Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and ..