Polymer Property : Transformation Temperature = -13.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature -25.0 °C
-13.0 °F
by DSC
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane
Features: Excellent clarity and UV stable with good melt strength. Pre-drying: 2 hours at 104°C (220°F) in dehumidifying hopper dryerUses: Extrusion: Cable jacket, hose/tube, profile and film and ..