Thermal Properties | Metric | English | Comments |
---|---|---|---|
Ring & Ball Softening Point | 163 °C | 325 °F | ASTM E28 |
Westlake Epolene® N-15 Nonemulsifiable - Low Molecular Weight Polypropylene Polymer Product Description: Epolene N-15 is a low viscosity polypropylene homopolymer with a high melt point and excellent hardness. Epolene N-15 is used in color concentrates, toner compounds, and as a pi.. |
|||
Ring & Ball Softening Point | 163 °C | 325 °F | ASTM E28 |
Westlake Epolene® N-15P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Description: Epolene N-15P is a low viscosity polypropylene homopolymer powder with a high melt point and excellent hardness. Epolene N-15P is used in color concentrates, toner compounds, and as a p.. |
|||
Ring & Ball Softening Point | 163 °C | 325 °F | ASTM E28-99 |
3M Scotch-Weld™ 3779 Hot Melt Adhesive High heat resistance; High strength; Good fuel and oil resistance and ElectronicsInformation provided by 3M |