Polymer Property : Ring & Ball Softening Point = 246 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Ring & Ball Softening Point 119 °C
246 °F
ASTM E28
Arkema Group EVATANE® 33-25 Copolymer Ethylene - Vinyl Acetate
EVATANE® 33-25 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-25 is stabilized with antioxidants. The High Vinyl Acetate co..
Ring & Ball Softening Point 119 °C
246 °F
ASTM E28
Arkema Group LOTADER® 6200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 6200 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Due to its properties (reactivity, fluidity), LOTADER 62..