Thermal Properties | Metric | English | Comments |
---|---|---|---|
Ring & Ball Softening Point | 119 °C | 246 °F | ASTM E28 |
Arkema Group EVATANE® 33-25 Copolymer Ethylene - Vinyl Acetate EVATANE® 33-25 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-25 is stabilized with antioxidants. The High Vinyl Acetate co.. |
|||
Ring & Ball Softening Point | 119 °C | 246 °F | ASTM E28 |
Arkema Group LOTADER® 6200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 6200 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Due to its properties (reactivity, fluidity), LOTADER 62.. |