Thermal Properties | Metric | English | Comments |
---|---|---|---|
Ring & Ball Softening Point | 132 °C | 270 °F | ASTM E28 |
DuPont Elvax® 350 Ethylene Vinyl Acetate DuPont™ Elvax® 350 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Addition: antiblock Applications:Elvax® 350 resins can be used for the following applications: .. |
|||
Ring & Ball Softening Point | 132 °C | 270 °F | ASTM E28-99 |
3M Scotch-Weld™ 3789 Hot Melt Adhesive High performance for plastics; Impact resistant; Bonds vinyl and wood and Good fuel and oil resistanceInformation provided by 3M |