DuPont Elvax® 350 Ethylene Vinyl Acetate

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Elvax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvax® 350 Ethylene Vinyl Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuPont™ Elvax® 350 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Addition: antiblock Applications:Elvax® 350 resins can be used for the following applications: molding, compounding and extrusion; wire and cable; and adhesives, sealants, and wax blends.Information provided by DuPont™
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ASTM D792-ISO 1183, ASTM D1505
Vinyl Acetate Content 25 %
25 %
Melt Flow 19 g/10 min

@Load 2.16 kg,
Temperature 190 °C
19 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
ASTM D2240-ISO 868
Hardness, Shore D 28
28
ASTM D2240-ISO 868
Thermal Properties Metric English Comments
Melting Point 74.0 °C
165 °F
ASTM D3417- ISO 3146
Vicat Softening Point 46.0 °C
115 °F
ASTM D1525, ISO 306
Ring & Ball Softening Point 132 °C
270 °F
ASTM E28
Descriptive Properties Value Comments
Cloud Point in Paraffin Wax, °C 66
10% Elvax® in fully refined paraffin wax, 146 AMP. Incompatible at temperatures up to 177°C.