Polymer Property : Clash Berg Stiffness Temperature = 6.11 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Clash Berg Stiffness Temperature 6.11 °C
43.0 °F
Dow Pellethane® 2103-90AEF Polyurethane Elastomer, Ether Based  (discontinued **)
PELLETHANE® 2103-90AEF elastomer is a polytetramethylene glycol ether based polyurethane elastomer, featuring superior resilience, low temperature properties, excellent hydrolytic stability, and re..
Clash Berg Stiffness Temperature 6.11 °C
43.0 °F
Dow Pellethane® 2103-90AEN Polyurethane Elastomer, Ether Based  (discontinued **)
PELLETHANE® 2103-90AEN is a polytetramethylene glycol ether based polyurethane elastomer featuring superior resilience, low temperature properties, excellent hydrolytic stability, and resistance to..