Thermal Properties | Metric | English | Comments |
---|---|---|---|
Clash Berg Stiffness Temperature | 6.11 °C | 43.0 °F | |
Dow Pellethane® 2103-90AEF Polyurethane Elastomer, Ether Based
(discontinued **) PELLETHANE® 2103-90AEF elastomer is a polytetramethylene glycol ether based polyurethane elastomer, featuring superior resilience, low temperature properties, excellent hydrolytic stability, and re.. |
|||
Clash Berg Stiffness Temperature | 6.11 °C | 43.0 °F | |
Dow Pellethane® 2103-90AEN Polyurethane Elastomer, Ether Based
(discontinued **) PELLETHANE® 2103-90AEN is a polytetramethylene glycol ether based polyurethane elastomer featuring superior resilience, low temperature properties, excellent hydrolytic stability, and resistance to.. |