Polymer Property : Clash Berg Stiffness Temperature = -40.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Clash Berg Stiffness Temperature -40.0 - -5.00 °C
-40.0 - 23.0 °F
Average value: -26.4 °C Grade Count:6
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
Clash Berg Stiffness Temperature -40.0 °C
-40.0 °F
Dow Pellethane® 2102-85A Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **)
PELLETHANE® 2102-85A elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with enhanced UV stability and good hydrolytic stab..
Clash Berg Stiffness Temperature -40.0 °C
-40.0 °F
At 10,000 psi (69 Mpa); ASTM D1043
Advanced Polymer Alloys Alcryn® 2070 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Clash Berg Stiffness Temperature -40.0 °C
-40.0 °F
At 10,000 psi (69 Mpa); ASTM D1043
Advanced Polymer Alloys Alcryn® 2070 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Clash Berg Stiffness Temperature -40.0 °C
-40.0 °F
69 Mpa; ASTM D1043
Advanced Polymer Alloys Alcryn® 2170 NC Melt Processable Rubber
Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades..
Clash Berg Stiffness Temperature -40.0 °C
-40.0 °F
At 10,000 psi (69 Mpa); ASTM D1043
Advanced Polymer Alloys Alcryn® 2060 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Clash Berg Stiffness Temperature -40.0 °C
-40.0 °F
At 10,000 psi (69 Mpa); ASTM D1043
Advanced Polymer Alloys Alcryn® 4660 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..