Thermal Properties | Metric | English | Comments |
---|---|---|---|
Clash Berg Stiffness Temperature | -20.0 °C | -4.00 °F | T-10000 Torsional stiffness ASTM D1043-72(1981) |
DuPont Performance Polymers Hypalon® 40 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound
(d Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato.. |
|||
Clash Berg Stiffness Temperature | -20.0 °C | -4.00 °F | At 10,000 psi (69 Mpa); ASTM D1043 |
Advanced Polymer Alloys Alcryn® 4670 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Clash Berg Stiffness Temperature | -20.0 °C | -4.00 °F | At 10,000 psi (69 Mpa); ASTM D1043 |
Advanced Polymer Alloys Alcryn® 4670 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |