Thermal Properties Metric English Comments
Transformation Temperature, Tg 441 °C
826 °F
Schott BG34 Conversion Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include FG3, FG13
Transformation Temperature, Tg 441 °C
826 °F
Schott SF2 Glass
Information Provided by SCHOTT North America, Inc.