Thermal Properties Metric English Comments
Transformation Temperature, Tg 645 °C
1190 °F
Schott N-SSK5 Glass
Information Provided by SCHOTT North America, Inc.
Transformation Temperature, Tg 645 °C
1190 °F
Schott S8806A Contrast Enhancement Filter
Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc.