Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 645 °C | 1190 °F | |
Schott N-SSK5 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 645 °C | 1190 °F | |
Schott S8806A Contrast Enhancement Filter Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 643 °C | 1190 °F | |
Schott N-LAK8 Glass Information Provided by SCHOTT North America, Inc. |