Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 599 °C | 1110 °F | |
Schott OG590 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, GG385, RG610, RG6.. |
|||
Transformation Temperature, Tg | 599 °C | 1110 °F | |
Schott N-PSK3 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 599 °C | 1110 °F | |
Schott KG1 Short Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG2, KG3, KG4, KG5 |
|||
Transformation Temperature, Tg | 599 °C | 1110 °F | |
Schott RG695 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |