Schott KG1 Short Pass Filter

Category Ceramic , Glass , Optical , Filter
Manufacturer Schott Glas Mainz
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott KG1 Short Pass Filter.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG2, KG3, KG4, KG5
Physical Properties Metric English Comments
Density 2.53 g/cc
0.0914 lb/in³
Thermal Properties Metric English Comments
CTE, linear 5.30 µm/m-°C

@Temperature -30.0 - 70.0 °C
2.94 µin/in-°F

@Temperature -22.0 - 158 °F
6.10 µm/m-°C

@Temperature 20.0 - 300 °C
3.39 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 599 °C
1110 °F
Optical Properties Metric English Comments
Refractive Index 1.53

@Wavelength 365 nm
1.53

@Wavelength 365 nm
Hg
1.53

@Wavelength 365 nm
1.53

@Wavelength 365 nm
Hg
Transmission, Visible 61 %

@Wavelength 700 nm
61 %

@Wavelength 700 nm
87 %

@Wavelength 500 - 510 nm
87 %

@Wavelength 500 - 510 nm
Internal transmittance of 94-95% from 480-580 nm.
87 %

@Wavelength 550 - 570 nm
87 %

@Wavelength 550 - 570 nm
Internal transmittance of 94-95% from 480-580 nm.
IR Transmittance 58 %

@Wavelength 710 nm
58 %

@Wavelength 710 nm
Internal transmittance of 63% at 710 nm.
UV Transmittance <= 0.020 %

@Wavelength 200 - 270 nm
<= 0.020 %

@Wavelength 200 - 270 nm
87 %

@Wavelength 370 - 390 nm
87 %

@Wavelength 370 - 390 nm
Internal transmittance of 95% from 380-390 nm
Reflection Coefficient, Visible (0-1) 0.92
0.92
Chemical Properties Metric English Comments
Acid Class, SR 2
2
Alkali Class, AR 3
3
Stain Resistance Class, FR 0.0
0.0