Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 585 °C | 1090 °F | ISO 7884-8 |
Schott G018-161 Dental Glass Remarks: Extremely high radioopacity, Zr containingApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provide.. |