Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Transformation Temperature, Tg = 1090 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature, Tg 586 °C
1090 °F
Schott GG420 Long Pass Filter
Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG385, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6..
Transformation Temperature, Tg 585 °C
1090 °F
ISO 7884-8
Schott G018-161 Dental Glass
Remarks: Extremely high radioopacity, Zr containingApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provide..
Transformation Temperature, Tg 590 °C
1090 °F
ISO 7884-8
Schott GM39923 Dental Glass
Remarks: Ba- and F-containing, low refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provide..
Transformation Temperature, Tg 590 °C
1090 °F
Schott N-LASF40 Glass
Information Provided by SCHOTT North America, Inc.
Transformation Temperature, Tg 589 °C
1090 °F
Schott N-SF6 Glass
Information Provided by SCHOTT North America, Inc.
Transformation Temperature, Tg 589 °C
1090 °F
Schott N-SF6HT Glass
Information Provided by SCHOTT North America, Inc.
Transformation Temperature, Tg 589 °C
1090 °F
Schott N-LAF35 Glass
Information Provided by SCHOTT North America, Inc.
Transformation Temperature, Tg 589 °C
1090 °F
Schott RG715 Long Pass Filter
Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6..