Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 535 °C | 995 °F | ISO 7884-8 |
Schott Glass 8449 Intermediate Sealing Glass Intermediate sealing glass Sealing to the glasses 8412, 8447, and 8487Information provided by SCHOTT AG. |
|||
Transformation Temperature, Tg | 535 °C | 995 °F | ISO 7884-8 |
Schott ILLAX® Amber Pharmaceutical Glass Amber Glass Pharmaceutical primary packaging for oralia and solid dosageInformation provided by SCHOTT AG. |