Material Notes:
Amber Glass Pharmaceutical primary packaging for oralia and solid dosageInformation provided by SCHOTT AG.
Physical Properties Metric English Comments
Density 2.50 g/cc

@Temperature 25.0 °C
0.0903 lb/in³

@Temperature 77.0 °F
Thermal Properties Metric English Comments
CTE, linear 7.80 µm/m-°C

@Temperature 20.0 - 300 °C
4.33 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Transformation Temperature, Tg 535 °C
995 °F
ISO 7884-8
Softening Point 720 °C
1330 °F
Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3
Working Point 1050 °C
1920 °F
Viscosity 10<sup>4</sup> dPa s; ISO 7884-2
Annealing Point 540 °C
1000 °F
Viscosity 10<sup>13</sup> dPa s; ISO 7884-4
Optical Properties Metric English Comments
Transmission, Visible 60 %

@Wavelength 500 nm
60 %

@Wavelength 500 nm
70 - 80 %

@Wavelength 550 - 800 nm
70 - 80 %

@Wavelength 550 - 800 nm
IR Transmittance 35 %

@Wavelength 2800 nm
35 %

@Wavelength 2800 nm
<= 40 %

@Wavelength >=4150 nm
<= 40 %

@Wavelength >=4150 nm
40 - 47 %

@Wavelength 3500 - 4150 nm
40 - 47 %

@Wavelength 3500 - 4150 nm
53 %

@Wavelength 3300 nm
53 %

@Wavelength 3300 nm
70 - 80 %

@Wavelength 800 - 1500 nm
70 - 80 %

@Wavelength 800 - 1500 nm
80 - 85 %

@Wavelength 1500 - 2700 nm
80 - 85 %

@Wavelength 1500 - 2700 nm
Component Elements Properties Metric English Comments
Al2O3 7.0 %
7.0 %
B2O3 5.0 %
5.0 %
BaO <= 0.50 %
<= 0.50 %
CaO 1.0 %
1.0 %
Fe2O3 2.0 %
2.0 %
K2O 1.0 %
1.0 %
Na2O 12 %
12 %
SiO2 67 %
67 %
Chemical Properties Metric English Comments
Acid Class, SR 2
2
DIN 12116
Alkali Class, AR 2
2
ISO 695
Descriptive Properties Value Comments
Hydrolytic Resistance Class HGB 2
ISO 719
Type III
PH. Eur
Type III
USP
MnO2 (%) 5