Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 581 °C | 1080 °F | |
Schott KG3 Short Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG2, KG1, KG4, KG5 |
|||
Transformation Temperature, Tg | 581 °C | 1080 °F | |
Schott N-BAK4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 582 °C | 1080 °F | |
Schott N-BASF64 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 580 °C | 1080 °F | |
Schott N-SF15 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 581 °C | 1080 °F | |
Schott RG9 Band Pass Filter Colloidally/ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
Transformation Temperature, Tg | 580 °C | 1080 °F | |
Schott N-BAF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 584 °C | 1080 °F | |
Schott N-KZFS5 Glass Information Provided by SCHOTT North America, Inc. |