Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG2, KG1, KG4, KG5
Physical Properties Metric English Comments
Density 2.52 g/cc
0.0910 lb/in³
Thermal Properties Metric English Comments
CTE, linear 5.30 µm/m-°C

@Temperature -30.0 - 70.0 °C
2.94 µin/in-°F

@Temperature -22.0 - 158 °F
6.10 µm/m-°C

@Temperature 20.0 - 300 °C
3.39 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 581 °C
1080 °F
Optical Properties Metric English Comments
Refractive Index 1.51

@Wavelength 587.6 nm
1.51

@Wavelength 587.6 nm
He
1.53

@Wavelength 365 nm
1.53

@Wavelength 365 nm
Hg
Transmission, Visible 79 %

@Wavelength 700 nm
79 %

@Wavelength 700 nm
90 %

@Wavelength 500 - 580 nm
90 %

@Wavelength 500 - 580 nm
Internal transmittance of 97% at 550-570 nm
IR Transmittance 77 %

@Wavelength 710 nm
77 %

@Wavelength 710 nm
Internal transmittance of 86% at 710 nm.
UV Transmittance <= 0.90 %

@Wavelength 200 - 290 nm
<= 0.90 %

@Wavelength 200 - 290 nm
90 %

@Wavelength 390 nm
90 %

@Wavelength 390 nm
Internal transmittance of 97% at 390 nm
Reflection Coefficient, Visible (0-1) 0.92
0.92
Chemical Properties Metric English Comments
Acid Class, SR 2
2
Alkali Class, AR 4
4
Stain Resistance Class, FR 0.0
0.0